The photo shows serious warping (or curling) of my print from my old PEI sheet which was printed on my MK4 with my old heatbed. All four of the corners warped (only the worst corner is shown).

This has been a persistent problem for the last couple of years. Smaller models printed closer to the center of the bed are fine. Only bigger prints which approach the edges of the bed curl up.

I recently upgraded my MK4 to the MK4S. While I was at it, I replaced the heatbed and I bought a new PEI sheet. And even though the sheet was brand new, I did wash it thoroughly with warm water and Dawn dish soap before using it.

After running through the full calibration and reslicing my model for the new high-flow nozzle using the latest stable release of PrusaSlicer, I reprinted it with high expectations.

Unfortunately, I was disappointed. One of the corners warped. It wasn’t quite as severe as before, so that’s a slight improvement. The corner that did warp happens to be the same one shown in the pic.

Print Settings: Prusa MK4S printer (no enclosure) 0.4 mm high-flow nozzle 0.2 mm resolution 15% infill Prusament Army Green PLA

– Edit –

Wow, there are lots of good ideas here. Thanks everyone!

The things I’m going to try (in no paticular order).

  • Covering the printer with a cardboard box or insulation sheets to see if an enclosure would help.
  • Cutting a tiny relief across the sides on the first layer.
  • Adding a brim.
  • Slow down the first layer.
  • Spraying 3DLac on the corners

– Final Report –

I tried all of the above suggestions. Spraying 3DLac works! I will definitely keep this stuff in stock. Thanks again everyone!

  • silico_biomancer@lemmy.nz
    link
    fedilink
    English
    arrow-up
    3
    ·
    edit-2
    2 months ago

    Lots of great advice in this thread. To add to it:

    Warp happens because of uneven cooling causing long straight lines of plastic to pull stronger than the bed adhesion. Sticking it to the bed better has had lots of focus in this chat. But you can also try to influence those first two parameters.

    Other than breezes, Uneven cooling might be because those corners of your plate aren’t heating as efficiently—possibly they aren’t as insulated or the heating element just doesn’t reach there as strongly, causing cooler spots. The part itself may also be cooling too quickly there because of holes or channels, where a more evenly solid part might cool slower and more consistently.

    My favourite hack for reliable designs though, especially if you wanted to share them and don’t want other people to worry as much about the warp, is creating relief features to address the long straight lines issue. Basically, on long lines heading into corners like you have here, a couple of centimeters from the corner, create a one layer high thin cut across the long line such that the slicer will interrupt the continuous line there. Make it as thin as you can get the slicer to register. Usually 0.1mm is sufficient. This is usually small enough that it will still end up closed over in the final part, so it won’t be apparent as an actual gap, but it will result in significantly less strain pulling on that corner.

    • aquovie@lemmy.cafe
      link
      fedilink
      English
      arrow-up
      2
      ·
      2 months ago

      Warping being directly proportional to long straight runs was a major educational moment for me for modeling.

      Thin cuts in large flat sections and “wrinkles” in long walls have eliminated any threat of warping. You can also change the first layer fill direction to have shorter runs.

    • mcavoya@lemmy.worldOP
      link
      fedilink
      English
      arrow-up
      1
      ·
      2 months ago

      I need to make two more prints of this model. I will give the Thin Cut idea a try!

      • silico_biomancer@lemmy.nz
        link
        fedilink
        English
        arrow-up
        1
        ·
        2 months ago

        Never tried deeper, could probably do more. But first only ensures it’ll never affect the part strength. Good question, theoretically the higher layers will still pull on the end; but at least the first layer isn’t de-adhering purely because of its own horizontal shrink

  • Marafon@sh.itjust.works
    link
    fedilink
    English
    arrow-up
    1
    ·
    2 months ago

    I had these types of issues a lot before I built an enclosure for my printer. It’s like night and day difference being able to keep the ambient temperature consistent throughout the print. A brim can also help with this but the enclosure is the real answer.

  • Fuzzypyro@lemmy.world
    link
    fedilink
    English
    arrow-up
    0
    ·
    edit-2
    2 months ago

    3 things.

    1. Wash your build plate with soap and hot water. It helps more with adhesion than you think. Do not use glue stick or any adhesives on the plate. People report that it works but I always found significantly better results with just soap and hot water on pei with materials that adhere to pei well such as pla. Masking tape with adhesives might make a difference for materials that do not stick to pei.
    2. If you are designing the part or have any time with cad then put a tiny bevel chamfer on the surface that touches the build plate. Doesn’t meet to be large. Just something. It helps with cooling shrinkage and retraction of pla on the first layers.
    3. enclosure or still air will help but are not strictly needed for pla.

    Last thing I would do is maybe adjust your z-offset. It looks like it might be experiencing some elephants foot at the bottom. I would try raising the head just by about .10. Really though that is going to be fully determined by your first layer of course.

      • Fuzzypyro@lemmy.world
        link
        fedilink
        English
        arrow-up
        0
        ·
        2 months ago

        Hey OP, just so you do not waste time. I mis-spoke and told you the opposite of what you should do in the program. No bevel, I meant chamfer!

        I know it doesn’t make a lot of sense to make the surface area touching the build plate smaller but it is worth it since it provides relief from the layers above pulling when it is shrinking.

          • Fuzzypyro@lemmy.world
            link
            fedilink
            English
            arrow-up
            2
            ·
            2 months ago

            Not trying to be combative here but the tests you linked further support what I was saying. A small chamfer and I really mean small will have a similar effect once rendered in gcode to a fillet. If you have access to software to generate a fillet easily that is good too. That being said I would only do it for the outer rim.

            Either way the print looks like it is warping on the lowest layers and has elephants foot which is what I suspect is the biggest issue here.

            The steps I proposed are

            1. Wash the plate to help with adhesion
            2. raise z offset just a tiny bit
            3. if possible add a chamfer
            4. if adhesion is still a issue add a brim
            • silico_biomancer@lemmy.nz
              link
              fedilink
              English
              arrow-up
              1
              ·
              2 months ago

              I might have misunderstood you, sorry. Do you mean a fillet or chamfer on the corners? (ie rounding as viewed from the top?) Or do you mean a chamfer such that the part’s second layer is slightly wider than the first layer?

  • SpaceNoodle@lemmy.world
    link
    fedilink
    English
    arrow-up
    0
    ·
    2 months ago

    Surprised nobody’s suggested adding a brim. That’s always been the final missing ingredient for me even after following all the other advice present in this thread.

    • FauxLiving@lemmy.world
      link
      fedilink
      English
      arrow-up
      0
      ·
      2 months ago

      Brim and also ensure that the room doesn’t have any active cooling.

      A fan blowing on the print will cause corners (with a higher surface area) to cool faster and the contraction will result in curling. Another alternative would be to put a cardboard box over the printer to ensure the print stays warm while it’s printing.

      • mcavoya@lemmy.worldOP
        link
        fedilink
        English
        arrow-up
        1
        ·
        2 months ago

        Throwing a cardboard box over it is a cheap and easy test. I’ll give that a try!

        • FauxLiving@lemmy.world
          link
          fedilink
          English
          arrow-up
          2
          ·
          2 months ago

          They sell enclosures also if you want to be able to see the print… but it’s hard to beat free.

  • Imgonnatrythis@sh.itjust.works
    link
    fedilink
    English
    arrow-up
    0
    ·
    2 months ago

    I have these issues with PETG on my mk4s, but usually not pla.

    Brim is a must for the wide based prints.

    Consider printing a draftshield if possible as well.

    If this fails try a gluestick (I like elagoo)

    Cleaning with isopropyl? Try a different brand (for whatever reason the cheaper generic drug store 90% ones seem to work best imo)

    Not sure it would help with this, but satin sheet has been a game-changer for me.

    • roofuskit@lemmy.world
      link
      fedilink
      English
      arrow-up
      0
      arrow-down
      1
      ·
      2 months ago

      For adhesion issues clean with soap and water, not alcohol. Take your build plate to the kitchen sink and wash it.